- Electrochemistry and Battery Testing
- DC and AC characterization of a Vanadium Redox Flow Battery (VRFB) using a Pinflow 20 cm² test lab cell Battery - Application Note 71
- Determination of the diffusion coefficient of an inserted species in a host electrode with EIS, PITT and GITT techniques Battery - Application Note 70
- How to check and correct non-stationary EIS measurements using EC-Lab® (Part 2) Battery - Application Note 69-2
- How to check and correct non-stationary EIS measurements using EC-Lab® (part 1) Corrosion - Application Note 69-1
- In-situ electrochemical study of LiFePO4 electrodes by quartz crystal microbalance Battery - Application Note 68
- Sensor pulsed techniques: SWV, DPV & NPV Electroanalysis & Electrochemistry Sensor - Application Note 67
- Systems and EIS quality indicators - Whitepaper - Electrochemistry
- Studying batteries with Electrochemical Impedance Spectroscopy - Whitepaper - Electrochemistry & Battery
- Electrical characterization of a ceramic with MTZ-35 and HTSH-1100 test fixture Material Science - Application Note 1
- EIS measurements on a RDE Part I: Determination of a diffusion coefficient using the new element Winf Electrochemistry - Application Note 66
- THD: parameters affecting its value & comparison with other methods of linearity assessment Battery & Corrosion - Application Note 65
- EIS Quality Indicators: THD, NSD & NSR Battery & Corrosion - Application Note 64
- High current (DC and EIS) measurements on electrolyzers Electrolyzers - Application Note 63
- How to measure the ohmic resistance of a battery using EIS (EIS-high-frequency-internal-resistance) Battery - Application Note 62
- How to interpret lower frequencies impedance in batteries (EIS low frequency diffusion) Battery - Application Note 61
- Distribution of Relaxation Times (DRT): an introduction Battery - Application Note 60
- A comprehensive solution to address battery module/pack Energy Storage - Application Note 59
- Battery cycling with reference electrodes using the PAT-cell test cell Battery - Application Note 58
- Differential Coulometry Spectroscopy (DCS) Battery - Application Note 57
- Levich and Koutecký-Levich analysis tools: Electrochemical reaction kinetics measurement Kinetics - Application Note 56
- Interpretation problems of impedance measurements on time variant systems Battery & Corrosion - Application Note 55
- How to read EIS accuracy contour plots Electrochemistry & Battery - Application Note 54
- Precision and Accuracy in Coulombic Efficiency Measurements (High Precision Coulometry HPC) Battery - Application Note 53
- UFS-SEC: SpectroElectrochemical Cell for UV-Vis, NIR and IR measurement Spectroelectrochemistry - Application Note 52
- Supercapacitor characterization by galvanostatic polarization method (DC characterizations) Supercapacitor - Application Note 51
- EIS Mathematics #2 - (The simplicity of Laplace transform) Battery - Application Note 50-2
- EIS Mathematics #1 -The simplicity of complex numbers and impedance diagrams Battery - Application Note 50-1
- Potentio or Galvano EIS Battery - Application Note 49
- Inaccuracy of corrosion current determination in presence of ohmic drop Corrosion - Application Note 48
- Corrosion current determination with mass transfer limitation Corrosion - Application Note 47
- In situ measurements for shrinking/dilation in energy storage devices during cycling Battery - Application Note 46
- ZFit and multiple impedance diagram fitting (EIS Zfit) Battery & Corrosion - Application Note 45
- Equivalent model of electrochemical cell inc. ref. electrode impedance and potentiostat parasitics Battery - Application Note 44
- How to fit transmission lines with ZFit (EIS transmission lines) Battery - Application Note 43
- The modified inductance element $L_\text a$ Battery - Application Note 42
- CV Sim: Simulation of simple redox reaction (E) Part 2 Ohmic drop effect & double layer capacitance Kinetics - Application Note 41-2
- CV Sim: Simulation of the simple redox reaction (E) - Part I: The effect of scan rate Kinetics - Application Note 41-1
- Differential (Incremental) Capacity Analysis Battery - Application Note 40
- Electrochemical Noise Measurements Part III: Determination of the noise resistance Rn Corrosion - Application Note 39-3
- Electrochemical Noise Measurements: Part II: ASTM assessment on a real electrochemical system Corrosion - Application Note 39-2
- Electrochemical Noise Measurements Part I: ASTM assessment and validation of instrumental noise Corrosion - Application Note 39-1
- Dynamic resistance determination. A relation between AC and DC measurements? EIS & Battery - Application Note 38
- CASP: a new method for the determination of corrosion parameters (CASP Rp determination) Corrosion - Application Note 37
- VASP: an innovative technique for corrosion monitoring (VASP Rp determination) Corrosion - Application Note 36
- Application of the Capacitance - Voltage curve to photovoltaic cell characterizations (EIS & CV curve) Photovoltaic - Application Note 35
- Supercapacitors Investigations Part II: Time Constant (EIS characterization) Supercapacitor - Application Note 34
- Supercapacitors investigations Part I: Charge/discharge cycling (DC characterization) Supercapacitor - Application Note 33
- Fuel Cell Testing Part II: EIS characterization (EIS characterization) Fuel-Cell - Application Note 32
- Fuel Cell Testing Part I: Overview and I/E characterizations (IV characterization) Fuel-Cell - Application Note 31
- IMVS investigation on photovoltaic cell (IMVS) Photovoltaics - Application Note 30
- Ohmic Drop Part III: Suitable use of the ZIR techniques (Ohmic drop & ZIR techniques) Battery - Application Note 29
- Ohmic Drop Part II: Intro. to Ohmic Drop measurement techniques (Ohmic drop measurement) Battery - Application Note 28
- Ohmic Drop Part I: Effect on measurements (Ohmic drop effect on measurements) Battery & Corrosion - Application Note 27
- EC-Lab® & BCS-800 with BT-Lab® graphic customization Battery - Application Note 26
- Multi Pitting Corrosion (Pitting) Corrosion - Application Note 25
- Photovoltaic Characterizations: Polarization and Mott Schottky plot Photovoltaic - Application Note 24
- EIS measurements on Li-ion batteries EC-Lab® software parameters adjustment (EIS optimizations) Battery - Application Note 23
- Corrosion of reinforced concrete Corrosion - Application Note 22
- Measurements of double layer capacitance Battery & Corrosion - Application Note 21
- EIS pseudocapacitance Battery & Corrosion - Application Note 20
- EIS measurements with multi sine Battery & Corrosion - Application Note 19
- Staircase Potentio Electrochemical Impedance Spectroscopy (SPEIS) and automatic successive ZFit analysis Battery - Application Note 18
- Drift correction in electrochemical impedance measurements (EIS non stationarity) Battery - Application Note 17
- Simultaneous impedance measurements elements of a running cell stack in EC-Lab® Express (EIS pack) Battery - Application Note 16
- Two questions about Kramers-Kronig transformations (EIS Kramers-Kronig) Battery - Application Note 15
- ZFit and equivalent electrical circuits (EIS Equivalent Circuit) Battery - Application Note 14
- Instrument & Quartz Crystal Microbalance (QCM) coupling: Mass measurement during polypyrrol film deposition Electrochemistry - Application Note 13
- UV-Visible spectroscopy & electrochemistry coupling: Spectroelectrochemisty on polypyrrol film Electrochemisty - Application Note 12
- Calculation of the active surface of platinum (Fuel cell ECSA) Corrosion - Application Note 11
- Corrosion current measurement for an iron electrode in an acid solution (Tafel plot LPR) Corrosion - Application Note 10
- Linear vs. non-linear systems in impedance measurements (EIS linearity) Battery - Application Note 9
- Impedance, admittance, Nyquist, Bode, Black, (EIS plot) Battery - Application Note 8
- Application of the bipotentiostat to an experiment with a Rotating Ring-Disk Electrode (RRDE bipot) Battery - Application Note 7
- Constant power technique and Ragone plot Battery & Electrochemistry - Application Note 6
- Precautions for good impedance measurements (EIS) Battery & Electrochemistry - Application Note 5
- The mystery of potentiostat stability explained (Potentiostat stability) Battery - Application Note 4
- Galvanostatic Cycling with Potential limitation 4: Low Earth Orbit (LEO) battery satellite protocol (GITT#2) Battery - Application Note 3
- Protocols for intercalation electrodes materials-2, Potentiodynamic Cycling/Galvanostatic Acceleration (PCGA) PITT Battery - Application Note 2
- Protocols for studying intercalation electrodes materials- I: Galvanostatic cycling/potential limitations (GCPL) GITT Battery - Application Note 1
- Material testing
- Photosynthesis
- Measurement of non-photochemical quenching using the JTS-150 pump probe spectrometerPhotosynthesis - Application Note 5
- Measurement of electrochromic bandshift at 520 nm with real-time scatter correction at 546 nmLife Sciences - Application Note 4
- Cyclic electron flow in C3 plantsPhotosynthesis - Application Note 3
- Cyclic and linear electron flow in plants revealed by JTS-10 spectrometerPhotosynthesis - Application Note 2
- The advantages of using green light to follow fluorescence changesPhotosynthesis - Application Note 1
- Rapid Kinetics and Spectroscopy
- Stopped-flow in the mid-IR using dual comb spectroscopy - AN38
- Which Quench Flow for my lab ? QFM & SFM Series - Quench flow - AN37
- Protein folding and Chevron plots - SFM Series - Stopped-flow - AN36
- Stopped-flow in cryogenic conditions using an external cryostat - Rapid Kinetics - Application Note 25b
- Membrane transport kinetics as measured by stopped-flow - SFM 2000 Series- µSFM- Rapid Kinetics - Application Note 35
- Well Plate Optical Characteristics Variation Effects on CD Measurements - EkkO - Spectroscopy - Application Note 34
- Global Concerns for CD Measurements using Well plates - Whitepaper - Spectroscopy
- UV cut offs due to volume and solution components - EkkO - Spectroscopy - Application Note 33
- Sensitivity Detection limits using proteinsEkkO - Spectroscopy - Application Note 32
- Reproducibility of CD measurements - EkkO - Spectroscopy - Application Note 31
- Allowed Sample types selected examples for CD measurements - EkkO - Spectroscopy - Application Note 30
- Evaporation Effects on Measurement Stability - EkkO - Spectroscopy - Application Note 29
- Meniscus and beam position effects on measurement stability EkkO - Spectroscopy - Application Note 28
- Getting the most from a 50 μl stock of sample using the μSFM for refolding experiments - μSFM - Rapid kinetics - Application Note 27
- Changing the way to do Circular Dichroism - MOS-500 - Spectroscopy - Application Note 26
- Stopped-flow in cryogenic conditions - SFM-2000 series - Rapid kinetics - Application Note 25
- Exciton coupled circular dichroism using MOS-500 - MOS-500 - Spectroscopy - Application Note 24
- DR-CD accessory for the determination of enantiomeric ratio - MOS-500 - Spectroscopy - Application Note 23
- Using MOS-500 for Magnetic Circular Dichroism - MOS-500 - Spectroscopy - Application Note 22
- Double mixing stopped-flow using interrupted flow method - SFM-2000 seriesRapid kinetics - Application Note 21
- Wide temperature range control -SFM-2000 series - Rapid kinetics - Application Note 20
- Automatic concentration dependance studies - SFM-2000 series - Rapid kinetics - Application Note 19
- High precision mixing ratios - SFM-2000 series - Rapid kinetics - Application Note 18
- Precise control of flow rate - SFM-2000 series -Rapid kinetics - Application Note 17
- High precision volume delivery - SFM-2000 series - Rapid kinetics - Application Note 16
- Submicrosecond dead time determination - SFM-2000 series - Rapid kinetics - Application Note 15
- ORD accessory - MOS-500 - Spectroscopy - Application Note 11
- Scanning probe workstations
- Sweep scan with Height Tracking Scanning Probes - Application Note 26
- SDS Reservoir Head Scanning Probes - Application Note 25
- Sweep scan in Scanning Kelvin Probe (SKP) experiments Scanning Probes - Application Note 24
- Ic-SECM - Bipolar Plates Scanning Probes - Application Note 23
- The use of the SVP470 for Vibrating Probe measurements of plants Scanning Probes - Application Note 22
- Using the SECM150 to Measure an NMC Battery Electrode Scanning Probes - Application Note 21
- Introduction to Foil Cell Scanning Probes - Application Note 20
- Investigation of the diffusion of ferricyanide through porous membranes using the SECM150 Scanning Probes - Application Note 19
- Achieving micron scale measurements using the SECM150 Scanning Probes - Application Note 18
- The use of height tracking SECM to measure mechanically exfoliated graphite Scanning Probes - Application Note 17
- Intermittent Contact (ic) SECM for relief of major topographic features Scanning Probes - Application Note 16
- Introduction to the USB-PIO: measuring the effect of light on a live leaf Scanning Probes - Application Note 15
- Introduction to the Modular Map Experiment: an Interdigitated Array electrode example Scanning Probes - Application Note 14
- Investigation of an interdigitated array electrode using ic-SECM Scanning Probes - Application Note 13
- 3D Map production using the 3DIsoPlot softwareScanning Probes - Application Note 12
- Measurement of a nano-patterned gold sample by ic-/ac-SECM Scanning Probes - Application Note 11
- dc- and ac-SECM Measurements on Si Nanowire Arrays Scanning Probes - Application Note 10
- SKP imaging example of a corroded Zn-plated Fe sample Scanning Probes - Application Note 9
- Graphical and analysis tools in M370/M470 software Scanning Probes - Application Note 8
- ac-SECM to investigate battery electrode materials in non-aqueous electrolyte Scanning Probes - Application Note 7
- Advantages of the intermittent contact SECM : two examples in corrosion Scanning Probes - Application Note 6
- Introducing the Microscopic Image Rapid Analysis (MIRA) software Scanning Probes - Application Note 5
- Post-treatment and optimization of area scan experiments Scanning Probes - Application Note 4
- SECM height relief with OSP: an application in sensors Scanning Probes - Application Note 3
- SECM height relief with OSP: An application in corrosion Scanning Probes - Application Note 2
- Height tracking with the SKP370 or SKP470 module Scanning Probes - Application Note 1