An oxygen delignified eucalyptus kraft pulp was bleached by applying a catalytic amount of a tertiary amine, 1,4-diazabicyclo[2,2,2]octane, and hypochlorous acid at varying pH, temperature, and time. The bleaching filtrate was analyzed for chloroform and AOX and the pulp for residual lignin, hexenuronic acid, and OX. In comparison with chlorine dioxide bleaching, the novel catalytic bleaching (pH < 6) generated only traces of chloroform and low contents of AOX and OX. Separate catalytic oxidations of authentic hexenuronic acid showed that it was a major precursor of chloroform. The results demonstrate a practical way to reduce organochlorine formation in pulp bleaching and provide new understanding on the reaction pathways that yield chloroform.

 

Read more

Need support ?

Work smarter. Not harder.

Subscribe to the newsletter and get more reads about this topic! Tech-tips, theory, latest functionality, new products & more.

Subscribe to the newsletter

No thanks!